Any ideas on preventing this type of corrosion or slowing it down. Mine are Eddelbrock heads but I guess the make is immaterial. The engine has not been run with coolant in it yet.
Any ideas appreciated.
I have installed a sacrificial anode, if only for mental health reasons.
HiI have installed a sacrificial anode, if only for mental health reasons.
Hi BrianMe, personally, I use 50% antifreeze mix, sacrificial anodes, anti seize on all head studs, numerous grounding straps, including one of those rubber ones that drags on the ground. Like the Irishman who wore two condoms; to be sure, to be sure!
These are rubber anti-static straps that attach to the frame of the vehicle and drag on the ground.Hi Brian
Tell me more about these grounding straps you use. Do you ground the engine direct or what? What material are the straps etc.
Cheers Marcus
Mike,
As in Martin?
Reverse osmosis water may not be your best choice. Water that has been striped of all it's elements will want them back and will go after the softest metal first. You want water with a neutral PH of 7. Any thing less is acidic, not good for aluminum heads. Anodes in the radiator will be a big help, zinc or magnesium is best along with the proper antifreeze. I used to work with DI ultra pure water and was amazed at how aggressive it was and how it rusted the best tools we had. Just my thoughts. Frank
Amazing, no work, no getting anything and cheap.Here's zinc anodes: https://www.boatzincs.com/engine.html
Hi
Are you using zinc or a zinc solution as an anode? If it is zinc how do you get it into contact with the aluminium and in the electrolyte as well?
Cheers Marcus