I have used glass bead in my machine in the past, and black beauty in another blaster that I tend to use outside. I just tried out aluminum oxide, (black), I believe it was 70 grit, from H Frt. What I found is, that is was very dusty, but it worked well on some light rust. Also, I found it was magnetic, which if it's non-ferrous, how could that be. Anyone have experience with different Almn. oxide media they can share.
I was experimenting with it because that's how the plating shop preps fasteners for Parkerizeing. Someone here mentioned that the Parkerizing they use rusted. The secret to a good durable finish is to heat Parkerized items in liquid grease or other lubricants which get's embedded in the finish. Thank you Fordbarners.
I was experimenting with it because that's how the plating shop preps fasteners for Parkerizeing. Someone here mentioned that the Parkerizing they use rusted. The secret to a good durable finish is to heat Parkerized items in liquid grease or other lubricants which get's embedded in the finish. Thank you Fordbarners.